Giorgio Armani S/S 2018
POY Oil:
Mixed this oil agent is into 10~15% emulsion, and the raw wire is oiled by the nozzle oiling method in the spinning process. Recommended oiling rate: 0.3~0.4%, it could reduce friction and static electricity, and improve the spinning efficiency.
POY Oil,Spinning finish for polyester filament POY, Pre-Oriented Yarn
NINGBO LUCKY CHEMICAL INDUSTRY CO., LTD , https://www.chinaluckychem.com